Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3EG7 - PA66-GF35 - BASF

Material Data Center offers the following functions for Ultramid® A3EG7:
unit conversion, PDF datasheet print, comparison with other plastics, application examples, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Glass fibre reinforced injection moulding grade for machinery components and housings with high stiffness and dimensional stability such as lamp socket housings, heating pumps, flow heaters as well as electrically insulating parts.
The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties
do not change.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 30 / * cm³/10min ISO 1133
温度 275 / * °C -
荷重 5 / * kg -
成形収縮率, 平行 0.5 / * % ISO 294-4, 2577
成形収縮率, 直角 1.0 / * % ISO 294-4, 2577
突き出し時の時の温度 195 °C -
機械的特性乾燥/調湿単位テスト基準
ISO データ
引張弾性率 11500 / 8500 MPa ISO 527
破壊応力 210 / 150 MPa ISO 527
破壊ひずみ 3 / 5 % ISO 527
引張クリープ弾性率, 1000h * / 6650 MPa ISO 899-1
シャルピー衝撃強さ, +23°C 95 / 107 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, -30°C 75 / 77 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C 14 / 22 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, -30°C 12 / - kJ/m² ISO 179/1eA
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10°C/min 260 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 250 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 260 / * °C ISO 75-1/-2
ビカット軟化温度, B 250 / * °C ISO 306
線膨張係数, 平行 22 / * E-6/K ISO 11359-1/-2
線膨張係数, 直角 93 / * E-6/K ISO 11359-1/-2
1.5mm厚さでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 1.6 / * mm -
Yellow Card 可用 はい / * - -
厚さhでの燃焼性 HB / * class IEC 60695-11-10
試験片の厚さ 0.8 / * mm -
Yellow Card 可用 はい / * - -
酸素指数 24 / * % ISO 4589-1/-2
電気的特性.乾燥/調湿単位テスト基準
ISO データ
比誘電率, 100Hz 4.3 / 10.1 - IEC 62631-2-1
比誘電率, 1MHz 3.8 / 4.5 - IEC 62631-2-1
誘電正接, 100Hz 120 / 1570 E-4 IEC 62631-2-1
誘電正接, 1MHz 210 / 830 E-4 IEC 62631-2-1
体積抵抗率 1E13 / 1E10 Ohm*m IEC 62631-3-1
表面抵抗率 * / 1E10 Ohm IEC 62631-3-2
耐電圧 39 / 37 kV/mm IEC 60243-1
耐トラッキング性 - / 550 - IEC 60112
その他の特性.乾燥/調湿単位テスト基準
吸水率 5 / * % Sim. to ISO 62
吸湿率 1.6 / * % Sim. to ISO 62
密度 1410 / - kg/m³ ISO 1183
材料特有の特性乾燥/調湿単位テスト基準
ISO データ
粘度数 145 / * cm³/g ISO 307, 1157, 1628
試験片の成形条件.単位テスト基準
ISO データ
射出成形, 樹脂温度 290 °C ISO 294
射出成形, 金型温度 80 °C ISO 294
射出成形, 射出速度 200 mm/s ISO 294
Processing Recommendation Injection Molding単位テスト基準
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.15 % -
樹脂温度 280 - 300 °C -
金型温度 80 - 90 °C -
機能
 粘度せん断速度. , Ultramid® A3EG7, PA66-GF35, BASF
 せん断応力-せん断速度. , Ultramid® A3EG7, PA66-GF35, BASF
 せん断弾性率-温度. , Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 せん断弾性率-温度. , Ultramid® A3EG7 (調湿), PA66-GF35, BASF
 応力-ひずみ. , Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 応力-ひずみ. , Ultramid® A3EG7 (調湿), PA66-GF35, BASF
 割線弾性率−ひずみ. , Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 割線弾性率−ひずみ. , Ultramid® A3EG7 (調湿), PA66-GF35, BASF
 応力-ひずみ (等時的). 23°C, Ultramid® A3EG7 (調湿), PA66-GF35, BASF
 クリープ弾性率−時間. 23°C, Ultramid® A3EG7 (調湿), PA66-GF35, BASF
クリープ曲線 23°C, Ultramid® A3EG7 (調湿), PA66-GF35, BASF
 応力-ひずみ (等時的). 60°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 クリープ弾性率−時間. 60°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
クリープ曲線 60°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 応力-ひずみ (等時的). 90°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 クリープ弾性率−時間. 90°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
クリープ曲線 90°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 応力-ひずみ (等時的). 120°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 クリープ弾性率−時間. 120°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
クリープ曲線 120°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 応力-ひずみ (等時的). 140°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 クリープ弾性率−時間. 140°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
クリープ曲線 140°C, Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 pvT , Ultramid® A3EG7, PA66-GF35, BASF
 引張弾性率-温度. , Ultramid® A3EG7 (乾燥), PA66-GF35, BASF
 引張弾性率-温度. , Ultramid® A3EG7 (調湿), PA66-GF35, BASF
特殊な特性
成形加工法.
射出成形.
納入形状.
ペレット.
添加剤.
滑剤., 離型剤.
特殊な特性.
熱安定化.
領域別の利用可能性
その他の情報
村遜速揃
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
耐薬品性
5wt%酢酸 (23゚C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com